Reduce bed temperature after 1st layer
Posted: 02 Aug 2016, 16:39
Hi,
I use Printbrite as a print surface to print ABS. Adherence is great and I don't experience any warping but it does require a hotter bed temperature for the first layer.
Is there a way to set a different bed temperature from the 2nd layer up?
Apologies if I missed something obvious.
Regards
Paul
Sent from my Nexus 7 using Tapatalk
I use Printbrite as a print surface to print ABS. Adherence is great and I don't experience any warping but it does require a hotter bed temperature for the first layer.
Is there a way to set a different bed temperature from the 2nd layer up?
Apologies if I missed something obvious.
Regards
Paul
Sent from my Nexus 7 using Tapatalk